<?xml version="1.0" encoding="UTF-8"?>
<!DOCTYPE ArticleSet PUBLIC "-//NLM//DTD PubMed 2.7//EN" "https://dtd.nlm.nih.gov/ncbi/pubmed/in/PubMed.dtd">
<ArticleSet>
<Article>
<Journal>
				<PublisherName>Gorgan University Of Agricultural Sciences and Natural Resources</PublisherName>
				<JournalTitle>Journal of Wood and Forest Science and Technology</JournalTitle>
				<Issn>2322-2077</Issn>
				<Volume>20</Volume>
				<Issue>4</Issue>
				<PubDate PubStatus="epublish">
					<Year>2014</Year>
					<Month>02</Month>
					<Day>20</Day>
				</PubDate>
			</Journal>
<ArticleTitle>The Comparison of Alkali and Boiling Water
Pretreated Bagasse APMP Properties</ArticleTitle>
<VernacularTitle>The Comparison of Alkali and Boiling Water
Pretreated Bagasse APMP Properties</VernacularTitle>
			<FirstPage>183</FirstPage>
			<LastPage>195</LastPage>
			<ELocationID EIdType="pii">1706</ELocationID>
			
			
			<Language>FA</Language>
<AuthorList>
</AuthorList>
				<PublicationType>Journal Article</PublicationType>
			<History>
				<PubDate PubStatus="received">
					<Year>2014</Year>
					<Month>07</Month>
					<Day>12</Day>
				</PubDate>
			</History>
		<Abstract>Alkaline Peroxide Mechanical Pulping (APMP) is an advanced process of basic &lt;br /&gt;Refiner Mechanical Pulping (RMP). The use of pretreatment on the raw material &lt;br /&gt;(especially nonwoody resources like bagasse), result in improving most of the pulp &lt;br /&gt;properties. This study was aimed to investigate the effect of pretreatment on the &lt;br /&gt;value of pulp yield, alkali absorbtion and handsheet properties of bagasse APMP. &lt;br /&gt;This especial bagasse was provided from Pars Paper Mill. The chemical &lt;br /&gt;compositions of bagasse and the characteristics of it&#039;s handsheets were determined &lt;br /&gt;according to the TAPPI standard rules. Bagasse was pretreated with boiling water &lt;br /&gt;and with 1% NaOH and 1% NaOH + 1% H &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;separately and in the same&lt;/span&gt; &lt;br /&gt;condition to provide pulp. Then the main treatment was done under this condition: &lt;br /&gt;  &lt;br /&gt;2% H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;at pH around 11, temp. 60 &lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: SymbolMT; font-size: small;&quot; lang=&quot;ZH-TW&quot;&gt;&lt;span style=&quot;font-family: SymbolMT; font-size: small;&quot; lang=&quot;ZH-TW&quot;&gt;&lt;/span&gt;&lt;/span&gt; &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;C, in three diffrent consistency. The duration&lt;/span&gt; &lt;br /&gt;of the main treatment was determined in the retention of 5% of the preliminary &lt;br /&gt;  &lt;br /&gt;H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt; &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;. The results indicated that, the highest values of alkali absorbtion, density and&lt;/span&gt; &lt;br /&gt;strength mechanical of the handsheets were obtained in the sample pretreated with &lt;br /&gt;  &lt;br /&gt;1% NaOH + 1% H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;in 10% consistency. The highest values of pulp yield and&lt;/span&gt; &lt;br /&gt;thickness of handsheets obtained from control sample bagasse and the highest &lt;br /&gt;  &lt;br /&gt;value of brightness obtained in the sample pretreated bagasse with boiling water in &lt;br /&gt;  &lt;br /&gt;20% consistency. In general, with increasing the value of alkali absorbtion by &lt;br /&gt;  &lt;br /&gt;bagasse, the pulp yield and the brightness of the handsheet decreased and their &lt;br /&gt;  &lt;br /&gt;strength mechanical increaced. &lt;br /&gt;  &lt;br /&gt; </Abstract>
			<OtherAbstract Language="FA">Alkaline Peroxide Mechanical Pulping (APMP) is an advanced process of basic &lt;br /&gt;Refiner Mechanical Pulping (RMP). The use of pretreatment on the raw material &lt;br /&gt;(especially nonwoody resources like bagasse), result in improving most of the pulp &lt;br /&gt;properties. This study was aimed to investigate the effect of pretreatment on the &lt;br /&gt;value of pulp yield, alkali absorbtion and handsheet properties of bagasse APMP. &lt;br /&gt;This especial bagasse was provided from Pars Paper Mill. The chemical &lt;br /&gt;compositions of bagasse and the characteristics of it&#039;s handsheets were determined &lt;br /&gt;according to the TAPPI standard rules. Bagasse was pretreated with boiling water &lt;br /&gt;and with 1% NaOH and 1% NaOH + 1% H &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;separately and in the same&lt;/span&gt; &lt;br /&gt;condition to provide pulp. Then the main treatment was done under this condition: &lt;br /&gt;  &lt;br /&gt;2% H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;at pH around 11, temp. 60 &lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: SymbolMT; font-size: small;&quot; lang=&quot;ZH-TW&quot;&gt;&lt;span style=&quot;font-family: SymbolMT; font-size: small;&quot; lang=&quot;ZH-TW&quot;&gt;&lt;/span&gt;&lt;/span&gt; &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;C, in three diffrent consistency. The duration&lt;/span&gt; &lt;br /&gt;of the main treatment was determined in the retention of 5% of the preliminary &lt;br /&gt;  &lt;br /&gt;H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt; &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;. The results indicated that, the highest values of alkali absorbtion, density and&lt;/span&gt; &lt;br /&gt;strength mechanical of the handsheets were obtained in the sample pretreated with &lt;br /&gt;  &lt;br /&gt;1% NaOH + 1% H &lt;br /&gt;  &lt;br /&gt;  &lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;O&lt;/span&gt;&lt;/span&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: xx-small;&quot;&gt;2 &lt;/span&gt;&lt;/span&gt;&lt;br /&gt;&lt;span style=&quot;font-family: Times New Roman; font-size: small;&quot;&gt;in 10% consistency. The highest values of pulp yield and&lt;/span&gt; &lt;br /&gt;thickness of handsheets obtained from control sample bagasse and the highest &lt;br /&gt;  &lt;br /&gt;value of brightness obtained in the sample pretreated bagasse with boiling water in &lt;br /&gt;  &lt;br /&gt;20% consistency. In general, with increasing the value of alkali absorbtion by &lt;br /&gt;  &lt;br /&gt;bagasse, the pulp yield and the brightness of the handsheet decreased and their &lt;br /&gt;  &lt;br /&gt;strength mechanical increaced. &lt;br /&gt;  &lt;br /&gt; </OtherAbstract>
		<ObjectList>
			<Object Type="keyword">
			<Param Name="value">Bagasse</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">APMP</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">Pretreatment</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">Yield</Param>
			</Object>
			<Object Type="keyword">
			<Param Name="value">Handsheet properties</Param>
			</Object>
		</ObjectList>
<ArchiveCopySource DocType="pdf">https://jwfst.gau.ac.ir/article_1706_405034678c2dc042589ca7343b1501b0.pdf</ArchiveCopySource>
</Article>
</ArticleSet>